Sign In | Join Free | My xpshou.com
xpshou.com
Products
Search by Category
1-10 Results for

pitting corrosion

from 1978 Products

High Pitting Corrosion Resistance Cold Rolled Stainless Steel Sheet Roll SUS304 SUS316 SUS316L

China High Pitting Corrosion Resistance Cold Rolled Stainless Steel Sheet Roll SUS304 SUS316 SUS316L on sale
High Pitting Corrosion Resistance Cold Rolled stainless steel sheet roll SUS304 SUS316 SUS316L 316L stainless steel is an austenitic stainless steel with excellent corrosion resistance and high-temperature strength. Its corrosion resistance is better than ......
Qingtuo Metal Products (Qingdao)Co.,Ltd

Address: Room101, Entrance 1, Building2, No.95 National Highway 204,Chengyang District , Shandong Province, China

Inconel Alloy Nickel Pipe with High Resistance To Acid Attack Pitting Corrosion Resistance and Melting Range 1332-1380 ℃

China Inconel Alloy Nickel Pipe with High Resistance To Acid Attack Pitting Corrosion Resistance and Melting Range 1332-1380 ℃ on sale
... corrosion. It is commonly used in chemical processing equipment, heat exchangers, and storage tanks. The high resistance to corrosion makes it ideal for use in harsh environments where other materials may fail. In addition to its corrosion resistance, the...
Changzhou DLX Alloy Co., Ltd.

Address: NO.32 West Taihu Road, Xinbei District, Changzhou, Jiangsu

Rusty Finish Corten Steel Fire Bowl , Round Steel Fire Pit Corrosion Stability

China Rusty Finish Corten Steel Fire Bowl , Round Steel Fire Pit Corrosion Stability on sale
Fire Pit Bowl The Corten Steel Fire Pit is the perfect low maintenance garden feature. Available in sizes from 60-150cm it is suitable for any sized space or budget! Starting out as a blue steel, as soon as Corten Steel is exposed to the elements it will ......
Wangstone Metal Sculpture Co., Ltd.

Address: Unit 701A, No. 837 Middle Qianpu 2nd Road, Siming District, Xiamen, China

Ferralium Alloy 255 (UNS S32550) ASTM A479 F60 Duplex Steel Bar With Pitting Corrosion Test ASTM G48 (Method A)

China Ferralium Alloy 255 (UNS S32550) ASTM A479 F60 Duplex Steel Bar With Pitting Corrosion Test ASTM G48 (Method A) on sale
... alloy with excellent corrosion resistance and high-temperature strength. The excellent impact resistance, good fatigue resistance, and high toughness of 03Cr25Ni6Mo3Cu2N give it significant advantages in ......
TSING SHAN STEEL INDUSTRIAL LIMITED

Address: NO.288,Youyi Road Xi Shan Dristrict , Wuxi, Jiangsu, China

Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar

China Ferritic Austenitic Duplex Stainless Steel Rod Pitting Corrosion Resistance 2507 Round Bar on sale
... of chromium and molybdenum, the steel has extremely high chromium and molybdenum content. Good resistance to pitting corrosion, crevice corrosion and uniform corrosion. The dual-phase microstructure ensures that the steel has a high resistance to stress...
Jiangsu Vespolari Steel Import & Export Co., Ltd.

Cold Rolled Bright ERNi-1 MIG Welding Wire Pitting Corrosion Resistance

China Cold Rolled Bright ERNi-1 MIG Welding Wire Pitting Corrosion Resistance on sale
SUS 316l stainless steel wires for making screw kitchen using ss 316L flat wire Description: Hot sell Bright MIG welding ERNi-1 wire ERNi-1 welding wire isused for welding of industrial pure nickel forgings and castings. Weling series:ERNiCrMo-3,ERNiCrMo......
Shanghai Haosteel Co., Limited

Address: No.581 Xiuchuan road, Pudong new area, Shanghai 201299, China

Steel Outdoor Fire Pit Garden Decor Corten Steel Fire Pit Table With Natural Rusty Colour

China Steel Outdoor Fire Pit Garden Decor Corten Steel Fire Pit Table With Natural Rusty Colour on sale
...Pit Garden Decor Corten Steel Fire Pit Table With Natural Rusty Colour Steel Outdoor Fire Pit lasts more than a lifetime: The Corten Steel body construction is extremely corrosion resistant and virtually invulnerable to the outdoor elements, protecting your backyard centerpiece for years to come. Say goodbye to bothersome smoke with the ultra-efficient airflow of our Steel Outdoor Fire Pit Garden Decor Corten Steel Fire Pit...
Gnee (Tianjin) Multinational Trade Co., Ltd.

Address: 25th Floor, Huafu Commercial Center, Wenfeng District, Anyang City,Henan Province

Outdoor Round Shape Wood Burning Corten Steel Fire Pit For Backyard

China Outdoor Round Shape Wood Burning Corten Steel Fire Pit For Backyard on sale
... alloy has been pre-oxidized to give it a stunning rusty orange, weathered appearance that is actually protecting it from further corrosive damage. It features a minimal low profile round design and is perfect for burning firewood on chilly nights as you...
Anyang Hongda Hydraulic Machinery Co., Ltd.

Address: Xiguzhuang Village,Shuiye Town,Anyang,Henan Province,China

Alloy 20cb3 Special Stainless Steel General Pitting Crevice Corrosion Resistance

China Alloy 20cb3 Special Stainless Steel General Pitting Crevice Corrosion Resistance on sale
... resistance to sulphuric and phosphoric acids Good resistance to intergranular corrosion Very good resistance to chloride-ion induced stress-corrosion cracking Good resistance to pitting and crevice corrosion Good mechanical properties at both ambient and...
Suzhou Xunshi New Material Co., Ltd

Address: Room E-407, No.2, XugongQiao Road, Kunshan City, Jiangsu, 215332 China

Nickel Alloy Flange ASTM B564 UNS N08825 Chemical Application Corrosion Resistance

China Nickel Alloy Flange ASTM B564 UNS N08825 Chemical Application Corrosion Resistance on sale
... strengthened corrosion-resistant alloy, the alloy contains high Ni and Cr elements, and at the same time a certain amount of Mo, Cu elements and stabilized Ti elements are added, so it has a good resistance to pitting corrosion, intergranular corrosion,...
Yuhong Group Co.,Ltd

Address: 20TH FLOOR,NO.1 NEW WORLD BUILDING ,NO.1018 MINAN ROAD,YINZHOU DISTRICT, NINGBO CITY, ZHEJIANG PROVINCE, CHINA

Submit your pitting corrosion inquiry in a minute :
*From:
Your email address is incorrect!
To:

Yuhong Group Co.,Ltd

Products: Nickel Alloy Flange ASTM B564 UNS N08825 Chemical Application Corrosion Resistance

*Subject:
Your subject must be between 10-255 characters!
*Message:
For the best results, we recommend including the following details:
  • --Self introduction
  • --Required specifications
  • --Inquire about price/MOQ
Your message must be between 20-3,000 characters!
 
Please reply me within 24 hours.
Yes! I would like your verified suppliers matching service!
Yes! If this supplier doesn't contact me in 3 days, I want everychina.com to recommend me more suppliers.
Submit pitting corrosion inquiry
*From:
Your email address is incorrect!
*Subject:
Your subject must be between 10-255 characters!
*Message:
For the best results, we recommend including the following details:
  • --Self introduction
  • --Required specifications
  • --Inquire about price/MOQ
Your message must be between 20-3,000
Yes! I would like your verified suppliers matching service!
Inquiry Cart 0